| PET-G | .020" | | PET-G | .020" | ||
| Acrylic | 1/8" - 3mm | 100% | 20mm/ | | Acrylic | 1/8" - 3mm | 100% | 20mm/ | ||
- | | ABS | 1/8" - 3mm | 75% | 20mm/s | | | + | | ABS | 1/8" - 3mm | 100% | 18mm/s | This previously said 20mm/s @75% but that wasn't cutting through |
| Felt | 1/16" | 10% | 20mm/ | | Felt | 1/16" | 10% | 20mm/ | ||
| Styrene | 0.30" | 100% | 20mm/ | | Styrene | 0.30" | 100% | 20mm/ | ||
- | | Acetate Film (Transparencies)| |10-15%|50mm/ | + | | Acetate Film (Transparencies)| |10-15%|50mm/ |
- | | Paper/Heavy Paper | -- | 5% | 50mm/s| | + | | Paper/Heavy Paper | -- | 5% | 50mm/s| | |
- | | Bristol Board | -- | 20% | 50mm/s| | + | | Bristol Board | -- | 20% | 50mm/s| | |
- | | Compact Disc | -- | 15% | 25mm/s| | + | | Compact Disc | -- | 15% | 25mm/s| | |
- | | EVA Foam | 1/2" | 100% | 40mm/s | | + | | EVA Foam | 1/2" | 100% | 40mm/ |
+ | | EVA Foam | "Hobby Foam" maybe 2mm? | 100% | 80mm/s | This may have been way overkill, but it was my first attempt and it worked fine but scorched the bottom a bit. | | ||
* Make sure the first pass cuts through or there will be too much smoke. The second pass is necessary because the plastic melts itself back together during the first pass. | * Make sure the first pass cuts through or there will be too much smoke. The second pass is necessary because the plastic melts itself back together during the first pass. |